Evening everyone,
Was going over everything before my big trip next week and noticed a crack in on of the welds in my procross bumper. Should I be concerned? Will it be OK to use on my trip or should I pull it off and put the stock one back one?
Thanks in advance,
Chris
Was going over everything before my big trip next week and noticed a crack in on of the welds in my procross bumper. Should I be concerned? Will it be OK to use on my trip or should I pull it off and put the stock one back one?
Thanks in advance,
Chris
Last edited:
tapex_07
TY 4 Stroke Master
- Joined
- Feb 15, 2009
- Messages
- 1,160
- Reaction score
- 135
- Points
- 1,038
- Country
- USA
- Snowmobile
- '10 Nytro MTX SE IMPULSE 174x3
'14 Viper XTX SE MPI 159x14x1.25
'07 Apex RTX SC2 MPI 128x1
Looks like its already off.. Guessing the weight of the bumper with the vibes of riding caused the weld to crack. Have you hit anything with it out of the norm?
Chewy
Extreme
- Joined
- Oct 2, 2015
- Messages
- 69
- Reaction score
- 17
- Points
- 98
- Location
- Ontario
- Country
- Canada
- Snowmobile
- Arctic Cat XF7000
Nothing that I can recall, weak weld from the factory maybe? Are these bumpers steel or aluminum?
tapex_07
TY 4 Stroke Master
- Joined
- Feb 15, 2009
- Messages
- 1,160
- Reaction score
- 135
- Points
- 1,038
- Country
- USA
- Snowmobile
- '10 Nytro MTX SE IMPULSE 174x3
'14 Viper XTX SE MPI 159x14x1.25
'07 Apex RTX SC2 MPI 128x1
Its Aluminum.
Chewy
Extreme
- Joined
- Oct 2, 2015
- Messages
- 69
- Reaction score
- 17
- Points
- 98
- Location
- Ontario
- Country
- Canada
- Snowmobile
- Arctic Cat XF7000
Wonder if I should try and find someone to weld it back up
Nytros rule
Expert
- Joined
- Jan 30, 2011
- Messages
- 469
- Reaction score
- 161
- Points
- 348
- Location
- Rider Nation
- Country
- Canada
- Snowmobile
- 2014 Black Viper XTX
Wonder if I should try and find someone to weld it back up
Take it back and TELL THEM TO REPLACE IT, don't ask, we pay way too much for this s--t to put up with the poor quality (material, welds and products) in our after market stuff.
You bought Cat I bought Yamaha because WE expect quality from our sleds, we deserve it from the accessories we buy.
If we wanted crap we'ed be driving one of the other two.
Last edited:
Crap! just looked and same thing starting on mine further forward. Honestly you are going to need to weld it anyway. Needs alot of weld there and factory doesnt do that. China you know.
- Joined
- Nov 29, 2009
- Messages
- 1,230
- Reaction score
- 992
- Points
- 1,578
- Location
- sabattus, maine
- Country
- USA
- Snowmobile
- 76 exciter, 87 phazer, 89 bravo, 00 srx x3, 01 srx, 02/04 viper, 06 ape
Are these the sport bumpers? That sucks, I was planning on getting one. Guess I'll have to take a better look at aftermarket options
Mine is the Cat Bumper but they all have the same stingy welds filling big gaps and are all aluminum. Still way better than stock. Just count on rewelding down the line.
Chewy
Extreme
- Joined
- Oct 2, 2015
- Messages
- 69
- Reaction score
- 17
- Points
- 98
- Location
- Ontario
- Country
- Canada
- Snowmobile
- Arctic Cat XF7000
Wonder if I should just go out and buy the Skinz procross bumper. Seems like this is an issue across all the bumpers from Cat
Not sure about your area but we have lots of great welders here. Simple fix and will be MUCH better than new. Up to you though anything is better than the little loop stock bumper.
Chewy
Extreme
- Joined
- Oct 2, 2015
- Messages
- 69
- Reaction score
- 17
- Points
- 98
- Location
- Ontario
- Country
- Canada
- Snowmobile
- Arctic Cat XF7000
Trying to find someone right now
- Joined
- Nov 29, 2009
- Messages
- 1,230
- Reaction score
- 992
- Points
- 1,578
- Location
- sabattus, maine
- Country
- USA
- Snowmobile
- 76 exciter, 87 phazer, 89 bravo, 00 srx x3, 01 srx, 02/04 viper, 06 ape
Yeah if I already had the bumper I'd just get it welded. Since I'm looking to buy a bumper I'm going to have to do some research before I decide. I really like the looks of the OEMs though.
tapex_07
TY 4 Stroke Master
- Joined
- Feb 15, 2009
- Messages
- 1,160
- Reaction score
- 135
- Points
- 1,038
- Country
- USA
- Snowmobile
- '10 Nytro MTX SE IMPULSE 174x3
'14 Viper XTX SE MPI 159x14x1.25
'07 Apex RTX SC2 MPI 128x1
I have a B&M Burly Bumper waiting to go on my sled.
- Joined
- Nov 29, 2009
- Messages
- 1,230
- Reaction score
- 992
- Points
- 1,578
- Location
- sabattus, maine
- Country
- USA
- Snowmobile
- 76 exciter, 87 phazer, 89 bravo, 00 srx x3, 01 srx, 02/04 viper, 06 ape
When you get it installed can you post a picI have a B&M Burly Bumper waiting to go on my sled.
-
This site uses cookies to help personalise content, tailor your experience and to keep you logged in if you register.
By continuing to use this site, you are consenting to our use of cookies.